Sign In | Join Free | My himfr.com
Home > Soft Magnetic Alloys >

Cold Drawn Wire Soft Magnetic Alloys HiperCo50 Iron-Cobalt Alloy with High Saturation

Suzhou Xunshi New Material Co., Ltd
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now
    Buy cheap Cold Drawn Wire Soft Magnetic Alloys HiperCo50 Iron-Cobalt Alloy with High Saturation from wholesalers
     
    Buy cheap Cold Drawn Wire Soft Magnetic Alloys HiperCo50 Iron-Cobalt Alloy with High Saturation from wholesalers
    • Buy cheap Cold Drawn Wire Soft Magnetic Alloys HiperCo50 Iron-Cobalt Alloy with High Saturation from wholesalers
    • Buy cheap Cold Drawn Wire Soft Magnetic Alloys HiperCo50 Iron-Cobalt Alloy with High Saturation from wholesalers

    Cold Drawn Wire Soft Magnetic Alloys HiperCo50 Iron-Cobalt Alloy with High Saturation

    Ask Lasest Price
    Brand Name : XUNSHI
    Model Number : UNS R30005
    Certification : ISO 9001
    Price : Available per request
    Payment Terms : T/T, Western Union
    Supply Ability : 1000 kg per week
    Delivery Time : 45-60 working days
    • Product Details
    • Company Profile

    Cold Drawn Wire Soft Magnetic Alloys HiperCo50 Iron-Cobalt Alloy with High Saturation

    HiperCo50 Cold Rolled Strip Iron-Cobalt Soft Magnetic Alloys High Saturation Iron-Cobalt


    XUNSHI supplies HiperCo 50 cold rolled strip with minimum thickness of 0.05mm. We are among the several TOP suppliers in China who are able to make this thickness. Our customers are from worldwide including EU&US.


    XUNSHI has rich experience of supply HiperCo50 parts, machined and heat treated. What's more, we are able to help our customers to improve the design of product.


    Diameter: 0.2-5.0mm


    HiperCo50 is an iron-cobalt alloy used in magnetic components requiring high permeability at and above 15 kG (1.5 T) or high magnetic saturation.


    In fact Hiperco50 has the highest magnetic saturation of all soft-magnetic alloys and excels in application where this attribute is needed. Hiperco 50 maintains its strength after heat treating making it your best choice for application that experience high forces (e.g. rotating parts).


    Designation: A801 − 14:

    Standard Specification for Wrought Iron-Cobalt High Magnetic Saturation Alloys (UNSR30005 and K92650)


    Main Characters

    • Highest magnetic saturation in all soft magnetic alloys
    • High Curie point-980°C
    • High magnetostriction

    Applications

    • Special motors for the aerospace industry
    • Electromagnets for medical applications
    • Electrical generators
    • Specialty transformers
    • Pole pieces for electromagnets
    • Magnetic bearings
    • High magnetic flux devices and instruments

    Typical Composition

    ElementsCMnSiCoNbVFe
    Weight(%)0.0100.050.0548.750.051.90Remainder

    Available Forms

    • Forging Billet—Hot-worked and surface prepared by grinding.
    • Hot-Rolled Bar, Plate, and Strip—Hot-rolled, hot- rolled and acid cleaned, and hot-rolled and mechanically cleaned.
    • Cold-Finished Bars—Centerless ground.
    • Cold-Rolled Strip
    • Cold-drawn Wire
    • Machined part per customers' drawing and specification, heat treated or not heat treated.

    Cold Drawn Wire Soft Magnetic Alloys HiperCo50 Iron-Cobalt Alloy with High SaturationCold Drawn Wire Soft Magnetic Alloys HiperCo50 Iron-Cobalt Alloy with High SaturationCold Drawn Wire Soft Magnetic Alloys HiperCo50 Iron-Cobalt Alloy with High Saturation

    Chemical composition(%, wt)

    • C: 0.15 max
    • Mn: 1.0-2.0
    • Si: 1.2
    • P: 0.015
    • S: 0.015
    • Co: 39.-42.0
    • Cr: 18.5-21.5
    • Ni:15.0-18.0
    • Mo:6.5-7.5
    • Be: 0.001 max
    • Fe: balance

    Characters

    • Exceptional resistance to corrosion, stress corrosion cracking and hydrogen embrtittlement.
    • Good fatigue stregth.
    • The absence of aging in service.
    • The absence of magnetism.
    • Ability to be used over a wide range of temperatures, from liquid helium to about 500°C.
    • Perfect passivity in contact with human tissues.
    • The possibility of increasing the strength of parts by age hardening after forming, leading to strength levels unattainable with other materials.
    • The absence of brittleness at low temperatures (no transition temperature).
    • A maximum service temperature about 100°C higher than for stainless steels.
    • A corrosion resistance vastly superior to that of molybdenum containing stainless steels.
    • A very high yield strength that combined with a high elastic modulus in both tension and torsion, enables the storage and rapid release of large amounts of elastic energy.

    Applications

    • Aeronautical and aerospace equipment
    • Automotive ABS systems
    • Automotive injection systems
    • Electrical and electronic apparatus
    • Equipment for the chemicals and oil & gas industries
    • Flexible coupling
    • Pacemaker electrodes
    • Printer springs
    • Prostheses for osteosynthesis
    • Shaped springs (helical, etc…)
    • Surgical implants and medical instruments
    • Various diaphragms

    Forms of supply

    • Bar
    • Cold Rolled strip
    • Drawn and flat wire
    • Heavy plate
    • Wire rod
    Quality Cold Drawn Wire Soft Magnetic Alloys HiperCo50 Iron-Cobalt Alloy with High Saturation for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: Suzhou Xunshi New Material Co., Ltd
    *Subject:
    *Message:
    Characters Remaining: (0/3000)